Home | Survey | Payment| Talks & Presentations | Job Opportunities
Journals   A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Special Steel
1003-8620
2015 Issue 3
Behavior of Nonmetallic Inclusions in Ultra-Low Oxygen Steel 25CrMoVNi for High Speed Rail Axles during RH Refining Process
Wei Pengyuan;,Jiang Min;,Yang Die;,Wang Xinhua;,Sun Wei;,Wang Kaizhong;
..............page:1-4
Analysis and Optimization on Hot Metal KR Desulphurization Process by Response Surface Methodology
Wang Zhen;,Su Chunyang;,Pan Mingxu;,Zhu Guofu;,Zhu Xiang;,Li Jian;
..............page:5-8
Analysis on Capillary Crack Defect in Anchor Steel CM690 and Process Improvement
Ma Jianchao;,Shi Kewei;,Yang Xie;
..............page:17-20
Design and Optimization of 180 t Converter Oxygen Lance Nozzle
Liang Huikun;,Feng Lianghua;,Zhang Ankun;,Liu Guanglong;
..............page:23-26
Pilot Production of Φ110 mm ~ Φ150 mm Gear Steel 22CrMoH by 110 t EAF-LF-RH-CC-Continuous Rolling Flowsheet
Cao Yanguang;,Wang Maoqiu;,Xu Le;,Liu Jianhui;,Dong Han;,Hu Fangzhong;,Sun Wei;
..............page:27-29
Cause for Submerged Entry Nozzle Blocking during Casting of Aluminium Killed Steel SPHC and Control Process
Zhang Dajiang;,Wang Cuina;,Xiang Hua;,Wan Guoxi;,Zheng Fei;
..............page:30-33
Heat Treatment Process of 245 mm Heavy Plate of Steel S500Q-Z35 for Seat Ring of Hydro-Power Station
Tang Zhenglei;,Xu Shaopu;,Lu Yuezhang;,Li Zhongbo;,Gao Zhaohai;,Yang Yang;
..............page:34-37
Effect of Ladle Top Slag Modification Treatment on Inclusions in Ultra-Low Carbon Steel in 210 t BOF-RH-Slab CC Flowsheet
Zhou Yelian;,He Qi;,Deng Zhiyin;,Zhou Jianfeng;,Zhu Miaoyong;
..............page:38-42
Influence of V Content on Natural Ageing Properties of High Nitrogen Steel 20MnSi
Yang Jichun;,Zhang Jian;,Zhou Li;,Li Hongwei;
..............page:43-45
Effect of Fluorite Content on Crystallization Properties of Casting Mould Fluxes
Han Xiuli;,Pan Miaomiao;,Liu Lei;,Zhang Han;,Liu Lina;
..............page:49-53
Behavior of Precipitation in Φ47 mm × 8 mm Tube of Heat Resistant Steel TP310HCbN during Rupture Test at 700 ℃
Fang Xudong;,Wang Yan;,Fan Guangwei;,Xia Yan;,Wang Zhibin;,Han Peide;
..............page:61-63