zhong guo cai liao wang quan xin gai ban -- zhuan ye hua ge xing hua fu wu cheng wei zhu xuan lv
..............
page:35
Electro-chemical Corrosion of Building Reinforcing Steel in Service
WANG Guo-dong;WEI Ying-hui;HOU Li-feng;HU lan-qing;XU Bing-she
..............
page:68-69
Carbon Nanotubes Synthesized in-situ at Carbon-ethanol Interface by Pulsed-laser Ablation
CHEN Chang-xin;CHEN Wen-zhe
..............
page:64-67
The Service Life of Screw Taps of Superhard Mateirals
LENG Pei-yu
..............
page:45-47,51
Wear Resistance of ZrO2 / (W, Ti) C Ceramic Materials
HUANG Chuan-zhen;ZHANG Lei;SUN Gao-zuo;WANG Quan-fu;LIU Han-lian
..............
page:41-44
Preparation of Fe-Cu-C Powder Metallurgy Material by Warm Compaction
LI Jin-hua;NI Dong-hui;ZHU Quan-li;ZHANG Wen;SHAO Ming
..............
page:38-40
Forming Limit Diagram Analysis of Tailor Welded Blanks
YAN Qi;YU Ning-feng
..............
page:36-37,40
Fracture Behaviour of Au-Ti(-Y) Alloys with a Minimum of 99. 0 Mass Percent Au
YANG Qing-qing;XIONG Wei-hao;ZHANG Jie;LAN Yong-zhong;PAN Ming
..............
page:33-35
Technology for Producing Free-cutting Sulfur-containing Steel with Cored Wire Injection of Sulfur Addition
ZHANG Tie-jun;LI Pei-jie;CUI Xue-cheng;E Cheng-zhi
..............
page:30-32
Application of Metal-ceramic Functionally Gradient Material to Internal Combustion Engines
XING Shi-kai;LI Ju-xia;WU Li-xun;BU Rong-kai
..............
page:61-63
The Static Compressive Properties of Cellular Al and Cellular Al Alloy
ZHENG Ming-jun;HE De-ping
..............
page:57-60
Application of Abrasion Resistant Medium Chrome White Cast Iron to Slurry Pump
ZHU Bao-gang;ZHAO Ya-zhong;ZHANG Xiu-mei
..............
page:54-56
Dry Wear and Friction of Thermal Spraying Aluminium Bronze Coating against GCr15 Steel
Zhi Long;WANG Yao-hua;TAN Ye-fa;WU Xin-Yue;WANG Ji
..............
page:52-53,56
Corrosion Behavior in NaCl Solution of 15 % Fe-Mg Alloy Synthesized by Mechanical Alloying
WU Sheng-qin;ZHU Xin-kun;LUO Yi;LAI Hua;TANG Hai-lin
..............
page:48-51
Work Hardening Mechanism of ZGMn18Cr2Mo Superhigh Manganese Steel
YUAN Zi-zhou;Kuang Yi;CHEN Xue-ding;QIU Shan
..............
page:9-11,15
Improving Material Properties with Magnetic Treatment
LIN Jian;ZHAO Hai-yan;CAI Zhi-peng;LU An-li
..............
page:5-8
Progress in the Research of Corrosion and Protection of Magnesium Alloys
CHENG Ying-liang;CHEN Zhen-hua;WANG Hui-ming;WU You-wu
..............
page:1-4
Wear-corrosion Behavior of Cr-Fe-C Amorphous Electroplating Deposition
LI Min;LI Hui-dong;LI Hui-qi;SUN Dong-bai
..............
page:27-29,32
Creep Behavior of Welded Joints in Stainless Steel 0Cr18Ni12Mo2Ti
ZHANG Xin;QU Jin-shan;WANG Da-chun;LI Guang-ming
..............
page:24-26
Microstructure of Electron Beam Weld Joints between Cemented Carbide YG30 and Carbon Steel
ZHAO Xiu-juan;YANG De-xin;WANG Hao;TAKAZAWA Kohji;TAGASHIRA Kohsuke;YAMAMORI Hideaki
..............
page:21-23,26
Application of the Micro-shear Test to Selection of Welding Wires
QUAN Si-yong;LEI Bin-long
..............
page:19-20,60
Initial Oxidation of Uranium
Lu Lei;BAI Bin;ZOU Jue-sheng;TANG Shi-hong;XIAO Hong
..............
page:16-18
Super High Cycle Fatigue of High Strength Steels at a Frequency of 20 kHz
XUE Hong-qian;TAO Hua
..............
page:12-15