Growth mechanism of aligned bamboo-like CNTs prepared by thermal CVD
LI Gang;YU Zong-sheng;XU Xian-feng;School of Mechatronic Engineering;East China Jiaotong University;
..............page:1-4
Interfacial characteristics and corrosion resistance of SiCp/Al composites under different surface treatment of SiC particle
CUI Xia;ZHOU Xian-liang;OUYANG De-lai;LIU Yang;ZOU Ai-hua;Institude of Materials Science and Technology;Nanjing University of Aeronautics and Astronautics;School of Materials Science and Engineering;Nanchang Hangkong University;
..............page:5-9
Effect of annealing treatment on microstructure and magnetic property of Co/Cu multilayers
HU Jia-zhi;CHEN Leng;School of Materials Science and Engineering;University of Science and Technology Beijing;
..............page:10-14
Preparation of molybdenum alloy doped with Al2O3 by hydrothermal synthesis method
HU Ya-jie;XU Liu-jie;ZHOU Yu-cheng;LI Ji-wen;LIU Wei;WEI Shi-zhong;School of Materials Science and Engineering;Henan University of Science and Technology;Henan Engineering Research Center for Wear of Materials;Henan University of Science and Technology;State Key Laboratory for Mechanical Behavior of Materials;Xi’an Jiaotong University;
..............page:15-20
Effects of Gd addition on microstructure and creep properties of Al2O3f/ Mg-6Al-0.5Nd composites
WANG Wu-xiao;SHEN Qing;ZHANG Dong-jie;WANG Xiao-hong;School of Material Science and Engineering;Xi’an University of Technology;
..............page:21-25
Effect of strain on grain boundary character distribution in Ni-5 at%W alloy
LI Long-fei;CHEN Xing-pin;SUN Hong-fu;LI Xiao-guang;College of Materials Science and Engineering;Chongqing University;
..............page:26-30
Effects of high pressure heat treatment on micro-mechanical properties of Cr phase in CuCr50 alloy
ZHAO Jun;ZHAO Xiao-jie;REN Guo-zhu;LI Xin;WU Xiang-nan;GUO Liang;LI Hong-bo;SUN Yan-rong;School of Materials and Engineering;North China Institute of Aerospace Engineering;State Key Laboratory of Metastable Materials Science and Technology;Yanshan University;Jiangsu Jinggong Special Material Limited Company;
..............page:31-35
Microstructure and mechanical properties of aged Al-4.5Cu-0.6Mg(-0.3Si) alloys
WANG Chuan;CHEN Li-jia;CHE Xin;LI Feng;School of Materials Science and Engineering;Shenyang University of Technology;
..............page:36-40
Effect of magnesium contents on microstructure and electrochemical performances of Al-Ga-Mn anode alloys
LIANG Ming-gang;WEN Jiu-ba;HE Jun-guang;CHENG Dan-dan;School of Materials Science and Engineering;Henan University of Science and Technology;Henan Synergistic Innovation Center of Nonferrous Metal Generic Technology;
..............page:41-46
Effects of Mg on microstructure and electrochemical properties of Al-Zn-Sn anode alloys
HE Jun-guang;WEN Jiu-ba;SUN Le-min;School of Materials Science and Engineering;Henan University of Science and Technology;Henan Synergistic Innovation Center of Nonferrous Metal Generic Technology;
..............page:47-52
Micro-textures of high strength 2A97 Al-Li alloy plates
CHEN Zhong-wei;FAN Qin-ying;State Key Laboratory of Solidification Processing;Northwestern Polytechnical University;
..............page:53-57
Effects of thermal cycling process on microstructure and properties of spray-formed Al-27%Si alloy
ZHU Xue-wei;WANG Ri-chu;PENG Jian;PENG Chao-qun;LIU Wen-shui;School of Materials Science and Engineering;Central South University;
..............page:58-64
Micro-mechanisms of quenching residual stress reduction for 2A02 aluminum alloy under aging treatment
WANG Yan;PENG Tao;ZHANG Mai-cang;School of Materials Science and Engineering;University of Science and Technology Beijing;
..............page:65-70
Effects of heat treatment on creep age forming formability of friction stir welded 2A12 aluminum alloy sheet
LIU Da-hai;ZONG Chong-wen;LI Jun-chu;ZENG Long-fei;School of Aeronautical Manufacturing Engineering;Nanchang Hangkong University;
..............page:71-77
Influence of homogenization treatment on recrystallization microstructure and texture of Al-Mn aluminium alloy
SHANG Li-man;CHEN Xing-pin;LI Xiao-guang;MEI Lin;College of Materials Science and Engineering;Chongqing University;
..............page:78-82
Experiment of laser deposition shaping for TC4 alloy based on one point cladding
TIAN Feng-jie;GAO Qiang;SHANG Xiao-feng;SONG Jian-xin;School of Mechanical Engineering;Shenyang Ligong University;School of Mechanical and Electrical Engineering;Shenyang Aerospace University;
..............page:83-87
Investigation on crack generating and expanding of SPCD deep-drawing sheet during stamping deformation
ZHOU Le-yu;CUI Tian-hao;HE Jian-zhong;ZHANG Chao-lei;LIU Ya-zheng;School of Materials Science and Engineering;University of Science and Technology Beijing;Technology Center;Baotou Iron & Steel Group Co Ltd;
..............page:88-92
Effect of welding technology on welding residual stress in welding joints of Q690 steel heavy plate
CHEN Zhong-yi;MA Yong-lin;WANG Wen-jun;XING Shu-qing;LU Heng-chang;School of Material and Metallurgy;Inner Mongolia University of Science and Technology;Baogang Design and Research Institute;Baogang Northwest Venture Industrial Development Co Ltd;
..............page:93-98
Effect of heat treatment on microstructure and properties of laser-welded BTi-6431S alloy joints
WU Kai;YAO Wei;FAN Xiao-long;YOU Feng-hai;WANG Zhi-min;Beijing Hangxing Machinery Manufacture Limited Corporation;
..............page:99-103
Microstructure and corrosion resistance of laser welded joints for dissimilar steels
JING Cai-nian;FAN Ji-chao;WANG Hua;XU Shu-bo;LIU Peng;School of Materials Science and Engineering;Shandong Jianzhu University;Analysis and Testing Center;Shanghai University;
..............page:104-108
Properties and microstructure of welded joint of high strength thick plate S620Q bridge steel
LI Zhen-tuan;XING Shu-qing;MA Yong-lin;CHEN Zhong-yi;LU Heng-chang;HAN Na;School of Material and Metallurgy;Inner Mongolia University of Science and Technology;
..............page:109-114
Textures of normalized grain-oriented silicon steel plate and precipitation particle distribution in grains with different orientations
HE Cheng-xu;MENG Li;MA Guang;CHEN Xin;MAO Wei-min;School of Materials Science and Engineering;University of Science and Technology Beijing;Department of Electrical Engineering New Materials and Microelectronics;State Grid Smart Grid Research Institute;State Key Laboratory of Advanced Metals and Materials;University of Science and Technology Beijing;
..............page:115-120
Recrystallization behavior of X100 pipeline steel
ZHOU Feng;WU Kai-ming;KANG Yong-lin;CHEN Jian-xin;Hubei Collaborative Innovation Center for Advanced Steels;International Research Institute for Steel Technology;Wuhan University of Science and Technology;Hunan Valin Lianyuan Iron and Steel Co Ltd;School of Materials Science and Engineering;University of Science and Technology Beijing;
..............page:121-125
Effects of increasing nitrogen and reducing nickel on hot deformation behavior of 316 stainless steel
YANG Ji-chun;ZHOU Li;DONG Meng-yao;ZHANG Jian;LI Hong-wei;School of Materials and Metallurgy;Inner Mongolia University of Science and Technology;
..............page:126-131
Microstructural characteristic and mechanical properties of 15Cr-5Ni stainless steel
MENG Li;CHENG Kang;School of Materials Science and Engineering;University of Science and Technology Beijing;
..............page:132-137
Microstructure and properties of a new martensitic stainless steel for conical refiner disc plate
SUN Guo-dong;JIA He-ze;ZHANG Wen-xue;ZHOU Li;YIN Feng-shi;School of Mechanical Engineering;Shandong University of Technology;School of Chemical Engineering;Shandong University of Technology;
..............page:138-143
Formation mechanism of precipitation free zone and its effect on mechanical properties of a fine-grain and high-strength IF steel
ZHANG Hong-mei;JIA Hong-bin;DONG Hang;WANG Hong-bin;Liaoning Key Laboratory of Material Formation and Microstructure Property Control;University of Science and Technology Liaoning;Dongbei Special Steel Group Dalian High Alloy Wire Rod Co Ltd;
..............page:144-148
Effects of long term aging on microstructure and properties of heat insulation oil pipe steel
JIA He-ze;SUN Guo-dong;YIN Feng-shi;XUE Bing;School of Mechanical Engineering;Shandong University of Technology;School of Chemical Engineering;Shandong University of Technology;
..............page:149-153
Fabrication of 1100 /7075 /1100 aluminum alloy clad sheet by hot roll bonding and heat treatment
CHEN Ze-jun;LIU Qing;WANG Guo-jun;WANG De-man;College of Materials Science and Engineering;Chongqing University;Northeast Light Alloy Co Ltd;
..............page:154-158
Quantitative characterization of lamellar microstructure in ultra-high strength pearlitic steel wire during cold drawing
WU Yong-gang;ZHOU Zheng;YANG Ben;WANG Li-xin;LIU Qing;College of Materials Science and Engineering;Chongqing University;
..............page:159-163
Influence of ion source pretreatment on WC substrate surface and Ta buffer coating
WEI Jun-jun;ZHU Xiao-yan;CHEN Liang-xian;LIU Jin-long;HEI Li-fu;LI Cheng-ming;ZHANG Yong;Institute for Advanced Materials and Technology;University of Science and Technology Beijing;Institute of Mechanics;Chinese Academy of Science;
..............page:164-168
Effect of laser peening and shot peening on stress corrosion sensitivity of 304 stainless steel
LU Zhi-ming;SHI Lai-min;ZHU Shen-jin;TANG Zhi-dong;JIANG Ya-zhou;GAO Hong-gang;College of Mechanical Engineering;Zhejiang University of Technology;Zhejiang Provincial Key Laboratory of Special Purpose Equipment and Advanced Processing Technology;
..............page:169-173
TiB2 strip + TiC particles multiscale strengthing phase for ceramic composite coatings by plasma cladding
WANG Ke;CUI Hong-zhi;WEI Na;ZHANG Yan-feng;WANG Shu-feng;CHENG Gui-qin;School of Materials Science and Engineering;Shandong University of Science and Technology;Qingzhou Haidun Hydraulic Machinery Manufacturing Co Ltd;
..............page:174-180
Morphology and wear resistance of ceramic coating on surfaces of AZ91D alloy prepared by micro-arc oxidation
CHE Guang-dong;LIU Xiang-dong;School of Materials Science and Engineering;Inner Mongolia University of Technology;Key Laboratory of Materials Processing and Control Engineering of Inner Mongolia Autonomous Region;
..............page:181-184
Preparation of Co and Cr metal coatings,and Ni-Cr and Co-Cr alloy coatings by cathode plasma electrlytic deposition
QUAN Cheng;HE Ye-dong;Beijing Key Laboratory for Corrosion;Erosion and Surface Technology;University of Science and Technology Beijing;
..............page:185-190
Ni and Ni-Al2O3 nano-coatings prepared by the cathodic plasma electrolytic deposition
YI Quan-xiu;HE Ye-dong;Beijing University of Science and Technology;Beijing Key Laboratory of Corrosion and Abrasion and Surface Technology;
..............page:191-196
High temperature oxidation behavior of arc ion plated NiCoCrAlYSi coating on gun steel
ZHANG Jian;GUO Ce-an;LU Xu-dong;GUO Qiu-ping;School of Equipment Engineering;Shenyang Ligong University;School of Materials and Metallurgy;Northeastern University;Department of Military Representatives in 474 Factory;
..............page:197-201
Fabrication and characterization of Cu2ZnSnS4 thin films prepared by magnetron sputtering
HUA Zhong;MENG Xiang-cheng;SUN Ya-ming;YU Wan-qiu;LONG Dong;ZHANG Shou-qi;Key Laboratory of Functional Materials Physics and Chemistry of the Ministry of Education;Jilin Normal University;
..............page:202-205
Stress corrosion cracking behavior of X80 steel welded joint in Ku’erle simulated soil solution
XIE Fei;WANG Dan;WU Ming;SONG Jia-liang;College of Petroleum Engineering;Liaoning Shihua University;Zhejiang branch;CNPC Petro China Company Limited;
..............page:206-210+232
Sulfidation mechanism of FV( 520) B stainless steel in high temperature and high pressure environment
CHEN Feng-jun;DU Xiao-dong;LANG Jing-wei;ZHOU Dan;SHEN Jian;LIU Guang-fu;Department of Materials;Hefei University of Technology;
..............page:211-215
Microstructure and strengthening of low temperature carburizing layer for 316 austenitic stainless steel
MA Fei;PAN Lin;ZHANG Liang-jie;LI Peng;ZHU Yun-feng;YANG Min-hong;Wuhan Research Institute of Materials Protection;
..............page:216-221
Tribological behaviors of 45 steel against DC53 steel under dry sliding condition
XIE Shi-fang;ZHANG Lin-wei;WANG Wu-rong;LU De-ping;MAO Dan-dan;WEI Xi-cheng;Institute of Applied Physics;Jiangxi Academy of Sciences;School of Materials Science and Engineering;Shanghai University;Patent Examination Cooperation Jiangsu Center of the Patent Office;
..............page:222-227
Hot compression deformation behavior and processing map of Cu-Cr-Zr-Y alloy
CHAI Zhe;ZHANG Yi;LI Rui-qing;XU Qian-qian;TIAN Bao-hong;LIU Yong;College of Materials Science and Engineering;Henan University of Science and Technology;Collaborative Innovation Center of Nonferrous Metals;
..............page:228-232