Home | Survey | Payment| Talks & Presentations | Job Opportunities
Journals   A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Transactions of Materials and Heat Treatment
1009-6264
2014 Issue 5
Current status and trend on toughness improvement of coarse-grained heat-affected zone of high strength high toughness pipeline steels
LEI Xuan-wei;WU kai-ming;CHENG Lin;WEI Ran;ZHOU Feng;WANG Hong-hong;AN Zheng-yuan;International Research Institute for Steel Technology;Wuhan University of Science and Technology;
..............page:1-8
Effect of WC content on hot deformation behavior of Al2O3/Cu-WC composites
FENG Jiang;TIAN Bao-hong;ZHANG Yi;Liu Yong;LI Quan-an;School of Materials Science and Engineering;Henan University of Science and Technology;Henan Key Laboratory of Advanced Non-ferrous Metals;
..............page:9-13
Effect of semi-solid processing on glass forming ability and mechanical properties of (Zr0.60Ni0.22Al0.18)96Fe4 alloy
LI Chun-yan;KOU Sheng-zhong;ZHAO Yan-chun;YUAN Xiao-peng;CHEN Yan;YUAN Zi-zhou;State Key Laboratory of Gansu Advanced Non-ferrous Metal Materials;Lanzhou University of Technology;Key Laboratory of Non-ferrous Metal Alloys and Processing of the Ministry of Education;Lanzhou University of Technology;
..............page:14-19
LaMgNi hydrogen storage alloy prepared by spark plasma sintering
DONG Xiao-ping;PANG Yan-rong;WANG Qing;CHEN Jia-yi;WANG Cui-biao;College of Quality and Technical Supervision;Hebei University;
..............page:20-23
Growth behavior of intermetallic compounds on Sn-3.0Ag-0.5Cu/Cu interface
LI Shuai;YAN Yan-fu;ZHAO Yong-meng;XU Yuan-yuan;College of Material Science and Engineering;Henan University of Science and Technology;
..............page:24-28
Wettability between 304 austenitic stainless steel and window glass
CHEN Chang-jun;LIU Xing;WANG Xiao-nan;ZHANG Min;ZHANG Chao;LI Yang;BAO Yi-wang;WAN De-tian;Laser Processing Research Center;School of Mechanical and Electrical Engineering;Soochow University;Shagang School of Iron and Steel;Soochow University;School of Materials Science & Engineering;Anhui University of Technology;Key State Laboratory of Green Building Materials;China Building Material Academy;
..............page:29-33
Microstructure analysis of reactive detonation sprayed Ti-B-C-N ceramic coating
MA Jing;YAN Dong-qing;HU Jian-wen;ZHANG Xin;LI Yang;School of Material;Hebei University of Science and Technology;Hebei Key Laboratory of Material Near-Net Forming Technology;Hebei University of Science and Technology;
..............page:34-38
Effect of Al2O3 addition on composition and structure of CaZrO3 synthesized from ZrO2 and CaCO3
YOU Jie-gang;ZHANG Guo-dong;GAO Pei-liang;YANG Xiao-feng;LU Zhao-xin;College of High Temperature Materials and Magnesium Resource Engineering;Liaoning University of Science and Technology;Ying Kou Qing Hua Groups;
..............page:39-43
Effects of heat treatment on microstructure and properties of Mg-12Gd-3Y-Sm-0.5Zr alloy
FU San-ling;LI Quan-an;JING Xiao-tian;CHEN Jun;School of Materials Science and Engineering;Xi’an University of Technology;College of Physics and Engineering;Henan University of Science and Technology;School of Materials Science and Engineering;Henan University of Science and Technology;
..............page:44-48
Microstructure and fatigue crack behavior of Al-Mg-Si-Mn alloy die cast plates
HU Zu-qi;WAN Li;WU Shu-sen;LIN Chong;State Key Laboratory of Materials Processing and Die & Mould Technology;Huazhong University of Science and Technology;
..............page:49-53
Relationship between plastic anisotropy and texture in Al-Mg-Si alloy sheets
WANG Xiao-feng;GUO Ming-xing;CAO Ling-yong;ZHANG Ji-shan;ZHUANG Lin-zhong;State Key Laboratory for Advanced Metals and Materials;University of Science and Technology Beijing;
..............page:54-59
Precipitation strengthening behavior of Al-Sc and Al-Sc-Zr alloys
ZHOU Chang-bing;XUE Na;WANG Xiao-jiao;SONG Hui;LIU Wen-qing;Key Laboratory for Microstructure;Shanghai University;
..............page:60-63
Influence of T6 treatment on corrosion resistance of Mg-9Al-Zn-0.16La alloy
ZHANG Jin-ling;LIU Yang-li;ZHOU Jing;WANG She-bin;XU Bing-she;College of Materials Science and Technology;Taiyuan University of Technology;Key Laboratory of Interface Science and Engineering in Advanced Materials;Ministry of Education;Shanxi Research Center of Advanced Materials Science and Technology;
..............page:64-68
Effect of heat treatment on microstructure and fracture morphology of rolled Al-5Fe based alloy
FU Da-jun;HUANG Li-guo;College of Material Science and Engineering;Liaoning Technical University;
..............page:69-73
Hot deformation behavior and dynamic recrystallization of Cu-Cr-Zr alloy
ZHANG Yi;LI Rui-qing;XU qian-qian;TIAN Bao-hong;LIU Yong;LIU Ping;CHEN Xiao-hong;College of Materials Science and Engineering;Henan University of Science and Technology;Collaborative Innovation Center of Nonferrous Metals;College of Materials Science and Engineering;University of Shanghai for Science and Technology;
..............page:74-78
Influence of Si and Mg powders on foaming process of aluminum foams
ZHANG Min;CHEN Chang-jun;WANG Xiao-nan;School of Mechanical and Electrical Engineering;Soochow University;Shagang School of Iron and Steel;Soochow University;
..............page:79-84
Microstructure of Super304H austenitic heat-resistant steel after long-term aging
OU Ping;SUN Jian;CUI Zheng-qiang;YANG Chang-shun;School of Materials Science and Engineering;Shanghai Jiaotong University;Shanghai Power Equipment Research Institute;
..............page:85-91
Effect of aging treatment on electrochemical corriosion behavior of 254SMo stainless steel
MA Li-na;LI Jian-chun;FAN Guang-wei;LIANG Wei;WANG Yi-de;College of Material Science and Engineering;Taiyuan University of Technology;Technology Center of Taiyuan Iron and Steel Co Ltd;
..............page:92-96
Continuous cooling transformation behaviour and mechanical properties of hot rolled TRIP steel
YU Wei;WANG Xiao;CAI Qing-wu;HE Chun-yu;Research Institute of Metallurgical Engineering;University of Science and Technology Beijing;
..............page:97-103
Influence of electric current pulse treatment on eutectoid structure of hypoeutectic Fe-C alloy
HUANG Zheng-yang;CEN Qi-hong;LI Zhen-hua;WU Ying;ZOU Lei;School of Materials Science and Engineering;Kunming University of Science and Technology;National Engineering Research Center of Waste Resource Recovery;
..............page:104-108
Bainite formation control of 12Cr2Mo1R steel heavy plate in normalizing process
MENG Qing-yong;WANG Fu-ming;LI Chang-rong;CUI Guan-jun;TANG Zheng-lei;State Key Laboratory of Advanced Metallurgy;University of Science and Technology Beijing;School of Metallurgical and Ecological Engineering;University of Science and Technology Beijing;School of Materials Science and Engineering;University of Science and Technology Beijing;Iron and Steel Research Institute of NanyangHanye Special Iron and Steel Co Ltd;
..............page:109-114
Effect of quenching temperature on microstructure and properties of Fe-Cr-B-Al alloy
WU Zhan-Wen;CHENG Peng;FU Han-guang;College of Science;Armed Police Engineering University;School of Materials Science and Engineering;Beijing University of Technology;
..............page:115-118
Kinetics of high temperature isothermal phase transformation of Fe-0.47C-2.3Si-3.2Mn steel under high magnetic field
CHEN Jian-hao;ZHOU Xiao-ling;MENG Lan;LI Zeng;Faculty of Materials Science and Engineering;Kunming University of Science and Technology;
..............page:119-122
Effect of tempering temperature on mechanical properties of Q960 low carbon baninitic steel
XIE Bao-sheng;CAI Qing-wu;YU Wei;CAO Jia-ming;LI Rui;National Engineering Research Center for Advanced Rolling Technology;University of Science and Technology Beijing;
..............page:123-130
Effect of annealing time on microstructure and properties of hot rolled ultrafine grained metastable steel
LI Ji-guang;HUANG Hai-liang;ZHAO Kun;ZHANG Shao-yong;WANG Tie-jun;School of Materials and Metallurgy;University of Science and Technology Liaoning;Science and Technology Department;Angang Steel;
..............page:131-136
Microstructure and mechanical properties of an ultra high strength steel after direct quenching and partitioning process
WAN De-cheng;CHEN Yu-lai;CAI Qing-wu;Engineering Research Institute;University of Science and Technology Beijing;
..............page:137-142
Influence of thermal deformation temperature on microstructure and texture of 3%Si CGO silicon steel
MI Zhen-li;ZHOU Yuan-yuan;LI Zhi-chao;JIANG Hai-tao;LI Hui;Engineering Research Institute;University of Science and Technology Beijing;
..............page:143-147
Preparation technology of property gradient bainite-martensite-austenite ductile cast iron grinding ball
SUN Ting;SONG Ren-bo;WANG Xu;DENG Peng;WU Chun-jing;School of Materials Science and Engineering;University of Science and Technology Beijing;
..............page:148-153
Low cycle fatigue behavior of gray cast iron HT250
YUAN Yong-li;HE Guo-qiu;FAN Kang-le;SHE Meng;LU Qi;LIU Xiao-shan;ZHU Min-hao;School of Materials Science and Engineering;Tongji University;Shanghai Key Laboratory for R&D and Application of Metallic Functional Materials;Nation Traction Power Laboratory;Southwest Jiaotong University;
..............page:154-159
Influence of local surface strengthening on fatigue properties of components with holes of an A-100 steel
GAO Yu-kui;College of Aerospace Engineering and Applied Mechanics;Tongji University;
..............page:160-164
Effect of laser transformation hardening treatment on wear properties of wheel/rail steel
GUO Huo-ming;WANG Wen-jian;LIU Teng-fei;GUO Jun;LIU Qi-yue;Tribology Research Institute;Southwest Jiaotong University;
..............page:165-170
Fabrication and wear resistance of Al2O3-TiO2 non-skidding coating by plasma spraying
HU Chuan-heng;DU San-ming;NIU Yong-ping;ZHANG Yong-zhen;Henan University of Science and Technology;Key Laboratory for Material Tribology of Henan Province;
..............page:171-175
Effects of laser irradiation on microstructure and properties of boronized 65Mn steel
WANG Hong-yu;WU Zhi-kui;YUAN Xiao-ming;ZHAO Yu-feng;CHENG Man;School of Mechanical Engineering;Jiangsu University;
..............page:176-180
Wear behavior of W-Mo-C layer on Ti6Al4V alloy by the equipotential hollow-cathode glow discharge
CHEN Fei;College of Materials Science and Engineering;Beijing Institute of Petrochemical Technology;
..............page:181-185
In-situ synthesis of Ti(CN)/Fe composite coating and wear and corrosion resistance
ZHAO Jian-guo;LI Jian-chang;LIU Yang;HAO Jian-jun;SUN Wei-lian;MA Yue-jin;College of Mechanical and Electric Engineer;Agriculture University of Hebei;
..............page:186-190
Influence of hot dip galvanizing process on inhibition structure of IF440 steel
CHEN Bin-kai;ZHANG Qi-fu;HAO Xiao-dong;ZHONG Hai-feng;YU Gang-qiang;New Metallurgy Hi-Tech Group Co Ltd;National Engineering Laboratory of Advanced Coating Technology for Metal Material;
..............page:191-195
Hot temperature compression deformation behavior and constitutive equation of TA1 titanium
SU Juan-hua;HAN Ya-wei;REN Feng-zhang;WEI Shi-zhong;CHEN Zhi-qiang;School of Materials Science Engineering;Henan University of Science and Technology;Henan Collaborative Innovation Center of Non-ferrous Metal Generic Technology;Luoyang Ship Material Research Institute;
..............page:196-200
Thermodynamic analysis of nitrogenous ferrovanadium alloy prepared by liquid nitriding method
LIU Wen-juan;ZHU Rong;BAI Rui-guo;MA Rui-feng;LI Dong-ming;WANG Rao;School of Metallurgical and Engineering;University of Science and Technology Beijing;Chengde Iron and Steel Group Co Ltd;
..............page:201-206
Numerical simulation of temperature field and flow field of ferrite stainless steel in water-cooling condition
YANG Jing-jun;PANG Rui-peng;CHENG Guo-guang;State Key Laboratory of Advanced Metallurgy;University of Science and Technology Beijing;School of Metallurgical and Ecological Engineering;University of Science and Technology Beijing;
..............page:207-213
Temperature field simulation of flat-bulb steel in electromagnetic induction heating process and technology optimization
YUAN Si-yu;SONG Hua;WANG Xu;Angang Steel Company Limited Technology Centre;University of Science and Technology Liaoning;
..............page:214-218