Home | Survey | Payment| Talks & Presentations | Job Opportunities
Journals   A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Hebei Metallurgy
1006-5008
2013 Issue 5
APPLICATION OF WASTE HEAT RECOVERY NEGATIVE ENERGY DUST-COLLECTING FOR HIGH-TEMPERATURE GAS OF ELECTRIC FURNACE
Huang Yongjian;Jia Jianyong;Cao Xiuhai;Shen Zhaohui
..............page:4-6,61
DISCUSSION ABOUT INCREASING CONTENT OF MgO IN SINTER
Zuo Jingyu;Bai Xiongfei
..............page:1-3
RESEARCH ABOUT ELEMENTS SEGREGATION AND LOOSEN IN 20CrMnTi STEEL
Zhou Shuxin;Zhou Huifang;Zhou Libo
..............page:11-13
PROCESS PRACTICE TO IMPROVE CASTING ABILITY OF MOLTEN STEEL OF LOW-SILICON 20MnCrS5
Zhang Yong;Yang Fenggong;Yang Huafeng;Dong Daxi
..............page:24-25,54
INFLUENCE OF Zn LOAD ON PRODUCTION OF BLAST FURNACE
Lu Zhongyi;Liu Guowen
..............page:19-20
BREAKDOWN TREATMENT OF INVERTOR
Qin Yougang
..............page:45-47
PRODUCTION OF ROLLING FLAT STEEL FORCARGO HANDLING FORK IN SEMI-CONTINUOUS ROLLING LINE
Zhang Xiaohui;Hou Xianjun;Qi Qingjun;Yan Yan
..............page:37-38,71
PRODUCTION OF SPRING STEEL WITH CONVERTER CONTINUOUS CASTING AND CONTINUOUS ROLLING PROCESS
Zhang Liliang;Han Jinlei;Li Shaojie;Chen Hongwei
..............page:39-41
DEVELOPMENT OF UNIVERSE-PURPOSE PROGRAM BLOCK FOR ROLL SPEED REDUCTION
Zhou Kan;Xu Shuchen
..............page:50-51,49
PASS OPTIMIZATION FOR 530 MILL
Qi Qingjun;Hou Xianjun;Ma Guiwang;Zhang Xiaohui
..............page:42-44
CONTINUOUS CASTING PRODUCTION OF GCr15 BEARING STEEL
Fan Jiantong;Li Rongxiang
..............page:28-31
OPERATION PRACTICE IN THELATER STAGE OF COMPAIGN OF 580 m3 BLAST FURNACE
Li Bin;Liu Yanmin;Yuan Zhaofeng
..............page:21-23
PRACTICE TO REDUCE COKE RATIO OF BLAST FURNACE
Bai Xiongfei;Zuo Jingyu
..............page:78-80
APPLICATION AND IMPROVEMENT OF NON-DESTRCUTIVE TESTING
Xie Wenfa;Wang Huiqing
..............page:72-74
FAILURE ANALYSIS FOR 52CrMoV4 SPRING USED BY LOCOMOTIVE
Jiao Lilong;Hou Xianjun;Li Shaojie;Fan Yiding
..............page:64-66,36
PRACTICE TO REDUCE CONSUMPTION OF NATURAL GAS
Li Wei;Xie Wenfa
..............page:81-83
CONTROL HARMFUL ELEMENTS BEFORE IRON-MAKING WITH THE MOST ECONOMIC WAY
Li Jie;Bai Xiongfei;Zuo Jingyu
..............page:84-88
REASON ANALYSIS AND IMPROVEMENT FOR END SURFACE FRAGMENTATION
Han Jinlei;Zhang Liliang;Chen Hongwei
..............page:57-58,80
INCLUSION DEFECT ANALSIS AND IMPROVEMENT FOR GCr15 BEARING STEEL
Wang Jingang;Li Lei
..............page:62-63,18
IMPROVEMENT OF CONTROL SYSTEM OF FAST-PASSING CAR OF COOLING BED
Xu Shuchen;Zhou Kan
..............page:48-49
PRACTICE TO REDUCE THE LEVEL OF BANDED STRUCTURE OF CARBIDE IN GCr15 BEARING STEEL
Wang Shaodan;Xu Wei;Liu Jianpei;Xu Jianxia;Ma Guiwang;Zhang Xiaoyong
..............page:55-56,74
CAUSE OF SURFASE CRACKS ON CASTING BILLET OF S335J2 STEEL AND ITS CONTROL
Liu Bing;Wang Gongliang;Liu Ruining
..............page:52-54