Home | Survey | Payment| Talks & Presentations | Job Opportunities
Journals   A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Heat Treatment of Metals
0254-6051
2012 Issue 8
Effect of hot rolling process on microstructure density and mechanical properties of Fe-20Mn-3Cu-1.3C TWIP steel
LIU Haijun1;ZHU Dingyi1;HU Zhenming2;SONG Weitao1;PENG Xian1;LIU Longlong1
..............page:93-97
Effects of Cu2+ concentration on morphology of phosphate coating on steel and its growth mechanism
WANG Ruming;ZHANG Chi;YIN Ge;YANG Zhigang
..............page:41-45
Fracture analysis of H13 steel die case
GU Min;WANG Hongwei;ZHAO Shaofu;LI Shuangxi
..............page:118-121
Effect of heat treatment on microstructure and mechanical properties of Ti6242S alloy
WANG Chen1;2;MAO Xiaonan2;HAN Dong2;ZHANG Pingxiang2
..............page:33-35
Microstructure and mechanical properties of laser clad Ni-Cr-B-Si coating on copper alloy
LI Yangliang1;2;ZHAO Xiaojun1;2;CHEN Qingyu1;2;WANG Hongtao1;2;WANG Li1
..............page:62-65
Process of Ni-P alloy plating for 28CrMo steel
CHEN Xiaowen;ZHANG Defen;BAI Jianghu;LONG Fei;LONG Dan;LI Senlin
..............page:59-61
Aging properties of Cu-2.8Ni-0.7Si-0.15Mg alloy
WANG Junfeng1;JIA Shuguo1;2;CHEN Shaohua3;LIU Ping1;SONG Kexing1
..............page:12-15
Failure analysis of narrow electrics brush
LIU Yinglai 1;GAO Minhua 2
..............page:126-129
Influence of carbon content on microstructure and abrasive resistance of the low alloy wear resistant steels
GUAN Zhiqiang1;HUANG Weigang1;WANG Song2;LI Chen2;LI Longbin2
..............page:72-75
Effect of tempering temperature on high-cycle fatigue properties of 60Si2MnA spring steel
XU Qian1;2;HUI Weijun1;2;LONG Jinming1;LIANG Mei3;CHEN Hongwei3
..............page:8-12
Microstructure refinement of niobium microalloyed low carbon bainitic bar steel
YI Min1;2;WANG Guodong1;CHEN Tao2;WANG Lifeng2;TONG Qian2
..............page:68-72
Microstructure and mechanical properties of HR3C steel weld joints aged at high temperature
LI Taijiang1;LIU Fuguang1;CHEN Weiwu2;ZHU Jianhua3;WANG Caixia1;LIU Liying1;WANG Bo1
..............page:16-20
Antibiotic bioactive coatings on Ti surfaces by microarc oxidation technology
WANG Jing1;2;SUN Fenglian2;MENG Xiangcai2;CHEN Yuyi2
..............page:50-54
High temperature mechanical properties of 25Cr5MoA nitriding steel
ZANG Yue1;3;REN Xueping1;ZHAO Yanjun1;2;LI Shuxia1
..............page:30-33
Influence of Cu and Mn on pseudoelasticity of TiNi alloy
WAN Xiaojun;PENG Wenyi;GUO Qiyun
..............page:76-79
Heat treatment process of low strength pipeline steels for electric resistance welded pipe
LI Jianyi1;SHEN Liqun1;LIU Yanmei2;GU Hailong1;LU Guangping1;SUN Zhigang1;XIAO Furen2;LIAO Bo2
..............page:87-92
Induction hardening for 9Cr18Mo steel spool
TANG Weijian;LUO Yue
..............page:105-106
Effects of heat treatment on microstructure and corrosion resistance of new mooring chain steel
ZHANG Mande;CHENG Xiaoying;WANG Sizhen;WANG Dingkang
..............page:1-7
Influence of solution treatment temperature on microstructure and shear strength of Ti-6Al-4V alloy
FENG Guangyong;SHEN Qingyuan;PAN Wentao
..............page:38-40
Effects of heat treatment on microstructure and mechanical properties of 13MnNiMoR pressure vessel steel
MA Heng;PAN Wendong;ZHOU Ping;WANG Yuexiang
..............page:20-23
Wetting kinetics and kinematics of quenchant for steels
CHEN Chunhuai1;YAO Jihong1;ZHU Zuchang2
..............page:107-114
Microstructure of hot galvanized layer formed in Zn-Al-Si alloy bath
TU Hao1;LI Zhenfeng2;3;SU Xuping1;GAO Cuiping2;3;WANG Jianhua1;PENG Haoping3
..............page:54-58
Effect of subcritical quenching on mechanical properties of 45 steel for gear shaft
ZHANG Zhijian1;YANG Xiaolong2;XI Shengqi2;YAO Fan2;HUANG Mingzhi1;WU Hongjing2
..............page:98-101
Microstructure of La-TZM alloy doped with rare-earth oxide La2O3
WANG Pengzhou1;WANG Kuaishe1;ZHANG Zheng1;HU Ping1;LIU Renzhi1;2;KANG Xuanqi1;HE Huancheng1
..............page:80-82
Network structure heredity and harm to high carbon and chromium bearing steel
LI Wenzhu;MA Huixia;HUANG Lei;WANG Xiaofeng
..............page:36-38
Improvement of heating furnace for spade type metal parts thermoforming
CHEN Lidong1;FU Changzhi2;DENG Chunyan1;LI Yajing3;ZHANG Liang1
..............page:115-118
Heat treatment process of Ni-hard 4 cast iron
HUANG Suning
..............page:101-104
Failure analysis of a broken exhaust valve for marine diesel engine
CUI Liying1;CHEN Yuzhen1;LIU Sha1;CHEN Yuping1;HUANG Tianying2
..............page:122-125